Thulium and ytterbium-doped titanium oxide thin films deposited by ultrasonic spray pyrolysis

Abstract

Thin films of thulium and ytterbium-doped titanium oxide were grown by metal-organic spray pyrolysis deposition from titanium(IV)oxide bis(acetylacetonate), thulium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate) and ytterbium(III) tris(acetylacetonate). Deposition temperatures have been investigated from 300C to 600C. Films have been studied regarding their crystallity and doping quality. Structural and composition characterisations of TiO2:Tm,Yb were performed by electron microprobe, X-ray diffraction and Fourier transform infrared spectroscopy. The deposition rate can reach 0.8 μm/h. The anatase phase of TiO2 was obtained after synthesis at 400C or higher. Organic contamination at low deposition temperature is eliminated by annealing treatments.

0

Turn this paper into a lesson

ArcXiv compiles a structured reading guide from this paper's metadata: plain-English importance, contributions, prerequisite concepts, which sections to read first, flashcards, and a quiz. Grounded in the abstract, never invented.

Discussion (0)

Sign in to join the discussion.

Loading comments…