Domain wall roughness and creep in nanoscale crystalline ferroelectric polymers
Abstract
We report piezo-response force microscopy studies of the static and dynamic properties of domain walls (DWs) in 11 to 36 nm thick films of crystalline ferroelectric poly(vinylidene-fluoride-trifluorethylene). The DW roughness exponent ζ ranges from 0.39 to 0.48 and the DW creep exponent μ varies from 0.20 to 0.28, revealing an unexpected effective dimensionality of ~1.5 that is independent of film thickness. Our results suggest predominantly 2D ferroelectricity in the layered polymer and we attribute the fractal dimensionality to DW deroughening due to the correlations between the in-plane and out-of-plane polarization, an effect that can be exploited to achieve high lateral domain density for developing nanoscale ferroelectrics-based applications.
Turn this paper into a lesson
ArcXiv compiles a structured reading guide from this paper's metadata: plain-English importance, contributions, prerequisite concepts, which sections to read first, flashcards, and a quiz. Grounded in the abstract, never invented.