One of the most important methods of producing materials and oxide coating is plasma electrolytic oxidation (PEO). Coatings made on aluminum in PEO method have two allotropes of α-Al2O3 and γ-Al2O3. Coatings containing α-Al2O3 have more hardness and wear resistance; therefore, the main goal of the present study is to optimize aluminum oxide allotrope for increasing the ratio of α-Al2O3 in coating made with PEO method. Results of the present study shows that the optimum electrolyte compound for making highest phase of α-Al2O3 has 2.9 g/lit of KOH, 1.15 g/lit of Na4P2O7, and 0.34 g/lit of NaAlO2 and ratio of highest allotropic pick of α-Al2O3 to highest allotropic pick of γ-Al2O3 (in XRD test) in the optimum condition is 0.622 and hardness is 1648 Vickers.