Semimetal to semiconductor transition in Bi/TiO2 core/shell nanowires
Abstract
We demonstrate the full thermoelectric and structural characterization of individual bismuth-based (Bi-based) core/shell nanowires. The influence of strain on the temperature dependence of the electrical conductivity, the absolute Seebeck coefficient and the thermal conductivity of bismuth/titanium dioxide (Bi/TiO2) nanowires with different diameters is investigated and compared to bismuth (Bi) and bismuth/tellurium (Bi/Te) nanowires and bismuth bulk. Scattering at surfaces, crystal defects and interfaces between the core and the shell reduces the electrical conductivity to less than 5\,\% and the thermal conductivity to less than 25\,\% to 50\,\% of the bulk value at room temperature. On behalf of a compressive strain, Bi/TiO2 core/shell nanowires show a decreasing electrical conductivity with decreasing temperature opposed to that of Bi and Bi/Te nanowires. We find that the compressive strain induced by the TiO2 shell can lead to a band opening of bismuth increasing the absolute Seebeck coefficient by 10\,\% to 30\,\% compared to bulk at room temperature. In the semiconducting state, the activation energy is determined to |41.30.2|\,meV. We show that if the strain exceeds the elastic limit the semimetallic state is recovered due to the lattice relaxation.
Turn this paper into a lesson
ArcXiv compiles a structured reading guide from this paper's metadata: plain-English importance, contributions, prerequisite concepts, which sections to read first, flashcards, and a quiz. Grounded in the abstract, never invented.