High thermoelectric power factor of poly(3-hexylthiophene) through in-plane alignment and doping with a molybdenum dithiolene complex

Abstract

Here we report a record thermoelectric power factor of up to 160 μ W m-1 K-2 for the conjugated polymer poly(3-hexylthiophene) (P3HT). This result is achieved through the combination of high-temperature rubbing of thin films together with the use of a large molybdenum dithiolene p-dopant with a high electron affinity. Comparison of the UV-vis-NIR spectra of the chemically doped samples to electrochemically oxidized material reveals an oxidation level of 10%, i.e. one polaron for every 10 repeat units. The high power factor arises due to an increase in the charge-carrier mobility and hence electrical conductivity along the rubbing direction. We conclude that P3HT, with its facile synthesis and outstanding processability, should not be ruled out as a potential thermoelectric material.

0

Turn this paper into a lesson

ArcXiv compiles a structured reading guide from this paper's metadata: plain-English importance, contributions, prerequisite concepts, which sections to read first, flashcards, and a quiz. Grounded in the abstract, never invented.

Discussion (0)

Sign in to join the discussion.

Loading comments…