A new medium-entropy diboride (MEDB) (W1/3Re1/3Ru1/3)B2 has been synthesized by spark plasma sintering of elemental powders at 1600 oC. Despite the dissimilar structures of WB2, ReB2 and RuB2, the sintered MEDB consists of a single hexagonal ReB2-type phase (space group P63/mmc) with a relative density of 94.2% and an average grain size of 6.8 2.2 um. Structural refinement and electron microscopy measurements show that the W, Re, and Ru atoms occupy the same crystallographic site and are distributed uniformly in the lattice. The (W1/3Re1/3Ru1/3)B2 MEDB has Vickers hardnesses of 30.7 GPa at a load of 0.49 N and 20.5 GPa at a load of 9.8 N, which are comparable or higher than those reported for individual binary counterparts.

0

Turn this paper into a lesson

ArcXiv compiles a structured reading guide from this paper's metadata: plain-English importance, contributions, prerequisite concepts, which sections to read first, flashcards, and a quiz. Grounded in the abstract, never invented.

Discussion (0)

Sign in to join the discussion.

Loading comments…