Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy

Abstract

Bulk ferromagnetic amorphous Fe-Ni-P-B alloys in rod shape were formed by a rapid solidification technique. The largest amorphous specimen prepared had a diameter of ~2.5 mm and the corresponding cooling rate for the glass formation of this alloy system in our experiment can be estimate to be around 492.4 K/s by the method of finite-difference numerical calculation. This value is on the same order of magnitude as the critical cooling rate Rc of Fe40Ni40P14B6 alloy estimated by the method of constructing the continuous-cooling-transformation (CCT) curve. It is indicated that the heterophase impurities have been eliminated well in our experiment.

0

Turn this paper into a full lesson

ArcXiv compiles a staged curriculum from this paper: 8-12 lessons across beginner → advanced, synthesised section guides, visuals, flashcards, a quiz, exercises, and on-demand deep dives per section. Grounded in the abstract, never invented.

Discussion (0)

Sign in to join the discussion.

Loading comments…