Skip to content

Perpendicular Anisotropy and g-Factor of Sputtered Ni Films on Si(111) Studied by Angle-Dependent Ferromagnetic Resonance

Dushyant Singh, Tharundev V, Subha Maity, Subhavenkadesh SS, Vigneshwari SR, Krista R. Khiangte

cond-mat.mes-hall

Abstract

Ni films with thicknesses of 312 and 1011\,Å were grown on Si(111) by dc magnetron sputtering at room temperature and studied by atomic force microscopy, grazing-incidence X-ray diffraction, X-ray reflectivity, magnetometry and angle-dependent ferromagnetic resonance. Both films are polycrystalline fcc Ni with smooth surfaces, a bulk-like (111) lattice spacing and a saturation magnetization of ≈480{\approx}480\,emu\,cm−3^{-3}, and both are magnetized in plane. The angular dependence of the resonance field, from the film plane to the film normal, is described by a uniaxial anisotropy model with first- and second-order terms. From this model, g=2.160±0.005g = 2.160\pm0.005 and 2.101±0.0142.101\pm0.014 and effective perpendicular anisotropies of (6.0±0.4)×105(6.0\pm0.4)\times10^{5} and (4.5±0.6)×105(4.5\pm0.6)\times10^{5}\,erg\,cm−3^{-3} were obtained for the thinner and thicker film, respectively. The conventional analysis of only the in-plane and perpendicular resonances gives gg-factors that are lower by 0.02--0.04. The perpendicular linewidths give upper limits for the Gilbert damping of α≤0.030α\le 0.030 and ≤0.038\le 0.038.

Create a lesson

Metadata

Categories
cond-mat.mes-hall, cond-mat.mtrl-sci