Compositional Mapping of Martensitic and Magnetic Transitions in Ni-Fe-Ga Bulk Alloys and Microwires

L. Straka, P. Veřtát, L. Nulandaya, M. Eliáš, D. Salazar, O. Heczko, R. Varga

cond-mat.mtrl-sciarXiv:2611.24503

Abstract

Despite extensive research on Ni-Fe-Ga magnetic shape-memory alloys, the compositional dependence of their martensitic and magnetic transition temperatures remains unclear. We analyze published bulk-alloy data alongside two complementary microwire series. While the pooled data show no unique dependence on e/a, elemental-concentration analysis reveals that Ni and Fe are the primary compositional controls of Ms and Tc, respectively, within 26-28 at.% Ga: Ms = 43.6 cNi - 2079 K and Tc = 17.4 cFe - 30 K. At fixed Ga, this creates a trade-off: raising Ms generally lowers Tc and vice versa, making it difficult to keep both above room temperature. Around 25 at.% Ga, bulk data exhibit considerable scatter, partly attributable to gamma-phase formation. Glass-coated microwires produced by the Taylor-Ulitovsky method, in which the gamma phase has generally not been reported, extend the accessible composition range toward lower Ga contents. The Ni(73-x)Fe(x)Ga27 (x = 18-22) series and the Ga-rich Ni50Fe21Ga29 and Ni50Fe23Ga27 microwires broadly follow the corresponding bulk trends. Remarkably, Ni50Fe25Ga25 and Ni50Fe27Ga23 microwires depart sharply from these trends, combining Ms at or above room temperature with Tc > 395 K. Their functional potential is demonstrated by approximately 10% reversible strain in Ni50Fe27Ga23 microwire during thermal cycling under constant tensile stresses up to 200 MPa.

Create a lesson