Fabrication of Bi2212 Cross Whiskers Junction

Abstract

An intrinsic Josephson junction has been successfully fabricated without any micro-fabrication technique. Two Bi2212 whiskers were crossed with one another and joined by post-annealing. The inter-whisker electrical transport properties were measured by the four-probe method. The temperature dependence of resistance exhibited metallic behavior above TC. The resistance decreased to zero around 80K, corresponding to the superconducting transition. The current-voltage characteristics at 5K exhibited a small hysteresis and voltage jump, which can be explained by the intrinsic Josephson effect.