We have measured the thermoelectric power (S) of high purity single-walled carbon nanotube mats as a function of temperature at various hydrostatic pressures up to 2.0 GPa. The thermoelectric power is positive, and it increases in a monotonic way with increasing temperature for all pressures. The low temperature (T < 40 K) linear thermoelectric power is pressure independent and is characteristic for metallic nanotubes. At higher temperatures it is enhanced and though S(T) is linear again above about 100 K it has a nonzero intercept. This enhancement is strongly pressure dependent and is related to the change of the phonon population with hydrostatic pressure.
Create a lesson
Related papers
Local wave-packet spectroscopy of the Drude weight in Tomonaga-Luttinger liquids
Takayuki Yokoyama, Yasuhiro Tada
Pt-induced semimetallic transport and enhanced thermoelectric response in the half-Heusler alloy YNi0.5Pt0.5Bi
Vikas Chahar, Shivam Rathod, Lankun Wang et al.
A rigid commensurate host and a defect that switches: vacancies in the frustrated alternating spin-(1, 1/2) Heisenberg chain
R. L. Silva, R. C. Silva, A. R. Pereira
Putting a Temperature on Electron Correlation
Paul G. Graf, Florian Matz, Markus Penz et al.
Interlocked Vortex Order in the Frustrated A3V9Te13 Lattice (A=Cs,Rb)
Zilong Li, H. -Q. Yuan, Xiaoqun Wang et al.
Probing Deconfined Quantum Criticality Point on a Digital Quantum Computer
Mrinal Kanti Giri, Pinaki Sengupta