Oxygen isotope effect and phase separation in the optical conductivity of (La0.5Pr0.5)0.7Ca0.3MnO3 thin films

Abstract

The optical conductivities of films of (La0.5Pr0.5)0.7Ca0.3MnO3 with different oxygen isotopes (16O and 18O) have been determined in the spectral range from 0.3 to 4.3 eV using a combination of transmission in the mid-infrared and ellipsometry from the near-infrared to ultra-violet regions. We have found that the isotope exchange strongly affects the optical response in the ferromagnetic phase in a broad frequency range, in contrast to the almost isotope-independent optical conductivity above TC. The substitution by 18O strongly suppresses the Drude response and a mid-infrared peak while enhancing the conductivity peak at 1.5 eV. A qualitative explanation can be given in terms of the phase separation present in these materials. Moreover, the optical response is similar to the one extracted from measurements in polished samples and other thin films, which signals to the importance of internal strain.

0

Turn this paper into a full lesson

ArcXiv compiles a staged curriculum from this paper: 8-12 lessons across beginner → advanced, synthesised section guides, visuals, flashcards, a quiz, exercises, and on-demand deep dives per section. Grounded in the abstract, never invented.

Discussion (0)

Sign in to join the discussion.

Loading comments…