Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys
Qiang Li
Abstract
Ferromagnetic bulk amorphous Fe40Ni40P14B6 alloy rods with a diameter of 1.2 mm can be prepared by means of a rapid quenching technique. If a fluxing technique is also used, amorphous rods with a diameter as large as 2.5 mm can be synthesized. The critical cooling rate Rc for the glass formation Fe40Ni40P14B6 is estimated to be on the order of 100 K.s-1
Create a lesson
Related papers
A Gaussian process coarse-grained potential for Na-montmorillonite
Yalda Pedram, Yaoting Zhang, Laurent Brochard et al.
First-principles theory of phonon renormalization from nonlinear electron-phonon interactions
Florian Kluibenschedl, Matthew Houtput, Jacques Tempere et al.
Spin-Lattice Dynamics and Interactions in Magnonic Spinels
Hari Paudyal, Yuri Suzuki, Michael E. Flatté et al.
Magnon-Phonon Dynamics in Multidimensional Antiferromagnetic Oxides
Yogendra Limbu, Michael E. Flatté, Durga Paudyal
Strain-Induced Metal-to-Insulator Transition in Antiferromagnetic SrCrO3 Thin Films
S. Jöhr, A. Carta, J. Moreno et al.
Tuning the Coercive Field in Ferroelectric Hf0.5Zr0.5O2-Al2O3 Heterostructures via Interfacial Charge Dynamics
Marshall B. Frye, Chanyoung Kim, Jeong-Woo Sun et al.