Compaction of bulk amorphous Fe40Ni40P14B6 alloys
Qiang Li
Abstract
The consolidations of two bulk amorphous Fe40Ni40P14B6 alloy discs are performed via hot pressing for a short time in its supercooled liquid region under a pressure of ~1.2 GPa. When the consolidated temperature Ts is lower, the conjunction of two bulk amorphous Fe40Ni40P14B6 alloy discs cannot be achieved. Only when Ts get to the vicinity of 675 K, two amorphous Fe40Ni40P14B6 alloy discs have low viscosity enough to be fully fused together in a short time and the resulting compacts retain ~90% amorphous phase. To further improve the consolidated temperature Ts, a vast amount of crystallization will occur and result in the embrittlement of amorphous alloy.
Create a lesson
Related papers
Temperature dependence of the charge density from first principles: application to the (222) forbidden reflection in silicon
Jean Paul Nery, Raveena Gupta, Olle Hellman et al.
Coupled anisotropic weak topological states and Floquet mixed-parity altermagnetism in two-dimensional Su-Schrieffer-Heeger models
Kunyuan Feng, Xibin Liu, Chenchen Liu et al.
Grain Boundary Phase Transitions Enable Diffusionless Climb of Disconnections
Md Sharier Nazim, Giacomo Po, Nikhil Chandra Admal
3D Cloud Component Analysis of Atomic Structures
Pai Li
Benchmarking of Fast and Interpretable UF Machine Learning Potentials
Pawan Prakash, Sam Dong, Richard G. Hennig
Grain-Boundary Premelting in High-Entropy Transition Metal Carbides
Marium M. Mou, Caleb Schenck, Samuel E. Daigle et al.