Calorimetric Investigation of NdBa2Cu3Ox Single Crystals
U. Tutsch, P. Schweiss, R. Hauff, B. Obst, Th. Wolf, H. Wuehl
Abstract
The specific heat of Nd(Y)Ba2Cu3Ox single crystals without substitution of Nd for Ba has been measured for various oxygen contents. In comparison with YBa2Cu3Ox, the maximum attainable transition temperature of the crystals is about 4 K higher and shifted from x = 6.92 to x = 7.0, the highest possible oxygen content. In spite of the difference in the Tc(x) dependences, the jump in the specific heat DeltaC/Tc in both systems increases continuously being maximum at x = 7.0. Bond valence sum calculations based on neutron diffraction data point to a retarded generation of holes with increasing oxygen content in the Nd system and a different hole distribution between the chains and the planes in comparison to YBa2Cu3Ox accounting for the different behaviour of both systems.
Create a lesson
Related papers
High-Temperature Superconductivity of the Fe-Se-H compound
S. I. Bondarenko, A. A. Prokhorov, N. N. Galtsov et al.
Stabilization of Interband Phase Solitons in Two-Band Noncentrosymmetric Superconducting Rings
Yuriy Yerin, Boris Malomed, Stefan-Ludwig Drechsler et al.
Strain-driven orbital-selective reconstruction and bicollinear-to-stripe evolution in FeTe
Zhenfeng Ouyang, Yin Chen, Yi-Heng Tian et al.
Supercurrent detection and manipulation of topological phase transitions in Shiba-Majorana hybrid systems
Debika Debnath, Ioannis Ioannidis, Paramita Dutta et al.
Exact pair density wave in topological moire flat bands and universal superfluid stiffness
Zhengzhi Wu, Ming-rui Li, Hong Yao
Electrical manipulation of oxygen stoichiometry in multiterminal YBa2Cu3O7-δ junctions
Daniel Stoffels, Caio C. Quaglio-Gomes, Nicolas Lejeune et al.